05
2022
-
07
Environmental simulation tests can help identify in advance how changes in weather temperature affect flexible packaging.
Flexible packaging refers to packaging whose container shape can change after the product inside has been filled or removed. It includes a variety of pouches, boxes, sleeves, and envelopes made from materials such as paper, aluminum foil, fibers, plastic films, and their composites.
Soft packaging uses materials such as various types of films, and whether these film materials are being formed or applied in the future, they essentially cannot be separated from the element of "temperature"—especially in related packaging testing and inspection processes. Environmental Simulation Testing It is the primary performance testing item. So, how do the temperature differences caused by climate change affect flexible packaging? Let’s explore that below.
Everyone knows the principle of thermal expansion and contraction in everyday life—it also applies to flexible packaging. Among the various processes in our equipment—such as film blowing (cast film), printing, lamination, and bag-making—the most noticeable change often occurs with the rubber rollers: rollers that feel softer in summer become exceptionally hard during winter. Environmental Simulation Testing It is known that, When the rubber roller is soft, it retains better elasticity, allowing for a slight reduction in pressure during production—resulting in increased transfer rates of both glue and ink. However, in winter, when the rollers become particularly hard, you’ll need to adjust the pressure upward ever so slightly. In more severe cases, you may even have to check whether the roller is slipping, as this will inevitably lead to lower transfer rates of glue and ink. Through Environmental Simulation Testing These measured microscopic changes require us to proactively address and resolve them during both process design and actual production.
The materials we use—such as thin films, adhesives, inks, and solvents—are essentially chemical substances, all of which require careful handling. Environmental simulation testing, Generally, the surface activity of a material is positively correlated with temperature: the higher the temperature, the better the material's activity. And the greater the material's activity, the stronger its affinity for the surface—meaning the higher the affinity, the better the material's surface activity. Consequently, when the temperature rises above that of the adhesive or ink, the material's wettability improves significantly, while its affinity for the adhesive or ink also increases simultaneously. Therefore, from Environmental Simulation Testing Shows, This is especially evident in the compounding process: under identical material and machine-speed conditions, bubbles are extremely unlikely to form when operating in summer—but in winter, bubbling occurs much more easily. The reason lies in the fact that at lower temperatures, the surface activity of the materials decreases, meaning their inherent "inertness" increases. As a result, their compatibility naturally declines.
Changes in weather temperature can cause the temperature of adhesives and inks themselves to fluctuate, which in turn affects their workability depending on ambient temperature changes. In actual production, many manufacturers are increasingly focusing on viscosity control—but if they overlook the influence of temperature, their efforts will remain only a partial, one-sided pursuit. Therefore, it’s crucial to carefully consider these factors when handling such materials. Environmental Simulation Testing It's very necessary. Different resins may have varying temperature sensitivity ranges, but it’s an undeniable fact that temperature and viscosity are inversely related. We’ve previously conducted experiments measuring how the viscosity of a particular resin changes at different temperatures. Environmental Simulation Testing When testing the resin—whose viscosity is 2,300 (measured using a Zahn cup #4 in about 25 seconds) at an ambient temperature of 25°C—the viscosity increases to 3,000 (Zahn cup #4 takes roughly 32 seconds) at just 15°C. In other words, reducing the temperature by 10 degrees causes the viscosity to rise by nearly 7 seconds! Of course, in actual production, the differences in viscosity may not be as dramatic due to variations among different resins and the fact that solvents are often added to dilute them. However, it’s undeniable that viscosity does indeed fluctuate depending on room temperature. This is precisely why, even when we rely on viscosity controllers and strictly follow SOPs to maintain consistent viscosity levels, significant quality deviations can still occur. After all, while the viscosity readings remain stable, the solid content of our adhesives and inks may actually be shifting—leading to unintended changes in performance.
Moreover, as temperatures fluctuate, the actual temperatures of both the adhesive and the ink also change. Consequently, at lower temperatures, the adhesive and ink themselves require more heat to evaporate their solvents; conversely, in higher-temperature conditions, solvents evaporate much more readily. As an example, a friend once conducted an experiment showing that under 35°C conditions, a single glue tank could evaporate up to 3 kg of ethyl acetate per hour. Environmental Simulation Testing It can be seen that, Temperature has a significant impact on the evaporation efficiency of solvents—leading to dry plates in summer and non-drying issues in winter. Beyond changes in material activity, this phenomenon is also closely tied to the heat required for solvent evaporation.
Soft packaging materials, inks, and adhesives are all essentially polymer-based materials derived from petroleum. The primary processing method for films (excluding aluminum foil and paper) involves heating to melt the material, transforming granules from a solid state into a fluid. Once this processability is achieved, we proceed to cool and shape the material as needed, ultimately forming the desired film. (Note that the wide variety of film types and their specific functional requirements involve such extensive technical details that they can’t be covered here.) Environmental Simulation Testing Shows, After processing, the surface of the film becomes inert, but we still need to perform surface treatments like corona treatment. However, to enhance the film's processability and meet market demands, co-blending modifications are typically applied during production—inevitably introducing additives such as slip agents, anti-blocking agents, and antistatic agents. These additives are usually low-molecular-weight substances that remain trapped inside the film, essentially "contained" within its polymer matrix, much like how a glass bottle holds various items inside. When temperatures rise, these low-molecular-weight components become more active, while they “settle down” again at lower temperatures. If there are flaws in the formulation control or design during processing, this can directly affect the film’s performance: for instance, improper migration of these additives may lead to either excessive or insufficient release, ultimately causing the coefficient of friction to increase or decrease significantly. That’s why, in most cases, anti-blocking agents and slip agents used in film materials are distinct from one another. On the market, many anti-blocking agents incorporate fine inorganic powder particles to ensure reduced surface roughness and minimized sensitivity to ambient temperature changes.
In summary, the actual temperature significantly impacts our flexible packaging—provided that we proceed with Environmental Simulation Testing And Only by carefully and meticulously handling each step can we produce stable, high-quality products. (Source: Online)